Al2O3 | Fe2O3 | MgO | SiO2 | Na2O |
>99% | <0.1% | <0.5% | <0.2% | <0.05% |
Item | Value |
Kutorwa kwemvura (%) | <1 |
Kuwanda kwehuwandu (g/cm3) | 1.9-2.2 |
Chaiyo giravhiti (g/cm3) | >3.6 |
Kupisa kwekushanda.(max) (℃) | 1650 |
Zviripachena porosity (%) | <1 |
Kuoma kwaMoh (chiyero) | >9 |
Asidhi kuramba (%) | >99.6 |
Alkali resistance (%) | >85 |
Item | Value |
Kutorwa kwemvura (%) | <1 |
Packing density (g/cm3) | 1.9-2.2 |
Chaiyo giravhiti (g/cm3) | >3.6 |
Kupisa kwekushanda.(max) (℃) | 1650 |
Zviripachena porosity (%) | <1 |
Size | Kupwanya simba | |
kg/chidimbu | KN/particle | |
1/8" (3mm) | >203 | >2 |
1/4" (6mm) | >459 | >4.6 |
1/2" (13mm) | >877 | >8.7 |
3/4" (19mm) | >1220 | >12 |
1" (25mm) | >1630 | >16 |
1-1/2"(38mm) | >2340 | >23 |
2" (50mm) | >3460 | >34 |